新型碳包埋磁性载体的水热合成与表征
Synthesis and characterization of novel magnetic carrier with its composition of Fe3O4/carbon using hydrothermal reaction
以葡萄糖为碳原料,加入到油酸稳定的四氧化三铁纳米颗粒的水溶液中,在170摄氏度反应3 h,制备了碳包埋磁性纳米颗粒。所得纳米颗粒的平均粒径在100-200纳米之间,磁饱和性质为12.4 emu/g。所得Fe3O4/C纳米复合材料还用XPS, XRD, FT-IR和Mössbauer谱进行了表征。
a simple method to prepare the novel magnetic carrier based on carbon matrix has been built by heating the aqueous solution of glucose and oleic acid stabilized Fe3O4 nanoparticle at 170 C for 3 h. The results show that the surface hydrophobic modification of Fe3O4 nanoparticle is necessary to the successful synthesis of Fe3O4/C nanocomposition, and a possible formation mechanism of Fe3O4/C nanocomposition was presented. The influence of the reaction parameters such as the concentration of oleic acid stabilized Fe3O4 nanoparticle, the reaction time, etc. on the product was also investigated. In the typical reaction (2.5 g/L of oleic acid-stabilized Fe3O4 nanoparticle, 0.5 M of glucose), Fe3O4/C nanocompositions with the average diameter in the range of 100-200 nm were obtained and its saturation is 12.4 emu/g. In order to characterize Fe3O4/C nanocompositions, XPS, XRD, FT-IR, and Mössbauer spectra were employed.
郭会时、何农跃、郁颖蕾、王志飞
材料科学
纳米磁性颗粒载体,纳米复合物,水热合成,碳包埋磁性颗粒,合成
magnetic carriernanocompositionhydrothermal reactionFe3O4/Csynthesis
郭会时,何农跃,郁颖蕾,王志飞.新型碳包埋磁性载体的水热合成与表征[EB/OL].(2006-03-23)[2025-08-16].http://www.paper.edu.cn/releasepaper/content/200603-428.点此复制