本文对AZ31B变形镁合金进行了CO2激光焊接实验。获得了“未熔透”“熔池熔透”“小孔熔透”“过熔透”四种熔透状态的焊缝,其中“小孔熔透”状态的焊缝具有最佳焊接质量。用光电二极管对等离子体光信号进行了检测,并发现光信号随不同熔透状态而变化。当焊缝“熔池熔透”和“小孔熔透”是,平均信号强度A具有最小值。而信号标准差δ与平均信号强度A的比被定义为R值来描述等离子体的波动倾向。当焊缝在“熔池熔透”的时候R值最高。通过对等离子体光信号的平均信号强度A和R值的检测,“小孔熔透”状态能够成功被识别出来。

Sheets of AZ31B wrought magnesium alloy were welded by CO2 laser. Welds of “partial penetration”, “weld pool penetration”, “keyhole penetration” and “excessive penetration” were obtained, and the “keyhole penetrated” weld possessed the best quality. The light emission of welding plasma was monitored by photo-diode, and it was found that the photo-diode signal varied with different penetration statuses. When the welds were “weld pool penetrated” and “keyhole penetrated”, the average signal amplitude A reached its minimum value. R , which defined as ratio of average amplitude A and standard deviation δ of signal was introduced to describe the fluctuation tendency of plasma, and the ratio reached its maximum value (which meant the lowest plasma stability) when welds were “weld pool penetrated”. By detecting the minimum value of A and R , “keyhole penetration” can be differentiated from “weld pool penetration” and “excessive penetration”.

陈武柱、单际国、任家烈、张婧、谭稳达、雷祥

焊接、金属切割、金属粘接材料科学

Z31B变形镁合金,CO2激光焊接,等离子体光信号,熔透状态识别

Z31B Wrought Magnesium Alloy CO2 Laser Welding Light Emission of Plasma Penetration Status Recognition